IMPORTANT NOTEThis web page is part of a web site that is no longer actively maintained by anybody at ANU SRES. It has been left on the web due to its apparent popularity (every time we've removed it, people have complained within 24 hours), but is presented AS IS - attempting to contact any individual named on the page is likely to fail, and the SRES webmaster doesn't want to hear about such failures or entertain any communication about updating of the page's contents. You have been warned. |
Two of each of MDF untreated, HD3 untreated, MDF treated and HD3 treated were placed in a swellometer for twenty four hours to measure moisture sorption in water over that period.
The sample size was 60mmm 20mm and an aluminium blank was cut to fit the third dimension.